Filament guides
PETG not sticking to the bed?
If PETG is not sticking to the bed, note when it lets go. A line that gets dragged as soon as it goes down calls for a different check from a corner that lifts later. Identify your exact build plate first, then check the PETG build plate comparison below.
What does the failure look like?
The nozzle drags the first lines across the plate
Check first-layer calibration first. If lines stay rounded, leave gaps or follow the nozzle, confirm the correct plate is selected in the slicer and run the printer’s recommended first-layer calibration. Retest with a small single-layer patch. Stop if the nozzle scrapes the plate.
Only a corner or one area lifts
Check whether the problem follows the spot or the model. Clean the plate as its maker directs, then try the same small test patch in the affected area and elsewhere on the plate. If only one spot fails, recheck that area and bed levelling. If the first layer looks even but a sharp corner of the model lifts later, try a brim to give that corner more contact with the plate.
The whole part comes loose mid-print
Check for a lifted edge or nozzle contact. Stop the print and look at the last intact layers or review the printer recording if you have one. An edge that curled up can catch the nozzle as it passes. If the part has a small footprint and the first layer looked even, try a brim on the next attempt. If the nozzle repeatedly hits the part, follow your printer maker’s troubleshooting steps before restarting.
PETG build plate comparison
Use the manufacturer’s instructions for the exact plate, coating and filament you have. These examples show how cleaning and release can differ. On a dual-sided plate, check which side is approved for PETG and select that surface in the slicer.
| Build plate | Cleaning, release layer and removal |
|---|---|
| Smooth PEIPrusa smooth steel sheet | Clean. Wipe the cold sheet with about 90% isopropyl alcohol (IPA). Release layer. Prusa prefers a powder-coated sheet for PETG. If you use its smooth sheet, apply a thin layer of PVA glue stick to the cold surface. PETG can pull up the PEI coating during removal. Remove. Let the sheet cool fully, then lift it off the bed and gently flex it to release the print. |
| Textured PEIPrusa textured steel sheet | Clean. Wipe the cold sheet with about 90% IPA. Keep acetone off the textured coating. Release layer. Prusa lists its textured sheet for standard PETG without a glue stick. Check the supplier’s guidance for your particular blend. Remove. Let the sheet cool fully. The print may release by itself. If needed, lift the sheet off the bed and flex it gently. |
| GlassUltiMaker S-series glass plate | Clean. Take the cooled glass out of the printer. Wash it with lukewarm water and a non-abrasive sponge, then dry it before refitting. Release layer. UltiMaker recommends a thin coat of UHU glue stick for its PETG on glass to reduce the chance of chipping. Remove. Wait until the glass is fully cool. If the part still holds, UltiMaker describes dissolving the glue with lukewarm water on the cooled, removed plate. UltiMaker cleaning guide · UltiMaker PETG guide · UltiMaker glass removal guide |
Work through a first-layer check
Save your slicer profile and record the plate, filament series and nozzle size. Use the same test patch and change one setting at a time.
- Confirm surface compatibility. Read the plate maker’s PETG guidance, including any required separation layer. Prusa warns that PETG can adhere strongly enough to damage smooth PEI. A clean surface still needs the correct preparation for this material.
- Prepare the plate as instructed. Use its approved cleaning method and avoid touching the prepared print area. Cleaning products, coatings and release methods are surface-specific; do not assume that a solvent or glue recommended for another plate is suitable.
- Check first-layer calibration. Follow your printer’s levelling or calibration procedure. Excessively lowering the nozzle can damage the surface. Keep a record of adjustments and stop a test if the nozzle is scraping or the layer is clearly failing.
- Verify the material settings. Check nozzle and bed temperatures against the current filament label, the plate limits and the printer profile. Review the first-layer speed using the printer maker’s guidance. Change one setting before repeating the same small test.
Prusa’s first-layer guide explains surface preparation, calibration and its smooth-PEI warning. Use its model-specific adjustments only with the applicable equipment.
Match the bed temperature to the series
The PETG temperature table lists the verified supplier references for our range. Bambu Lab PETG Basic’s PEI reference, greatsimple PETG HF and Tinmorry PETG-ECO have different bed guidance. The verified R3D Off-White and Transparent 3kg label information gives a nozzle range; it does not establish a bed temperature. Check that roll’s current instructions.
Common questions
What if PETG is sticking too well?
Allow the plate to reach the removal condition specified by its maker and follow its release procedure. Avoid forcing the part off. If it will not release as instructed, ask the plate manufacturer for advice before using tools or chemicals. Check the preparation required before the next PETG print.
Should I keep increasing bed temperature?
Stay within the filament, surface and printer limits. Check the observations from your test first. Use the same model and compare one supported change, rather than changing temperature, calibration and speed together.
Could damp filament be involved?
Check filament condition if extrusion is also inconsistent. Popping or bubbles warrant investigation alongside your settings. Our PETG drying guide explains the available series references without treating those symptoms as proof of moisture.
For your next project, compare Bambu Lab PETG Basic refills or the current filament range. Check the product’s setup information and spool requirements alongside your printer and plate.